0.07% Pt/r.d-SnO2-ALD, 0.27% Pt/r.d-SnO2-ALD, 0.32% Pt/r.d-SnO2-ALD粉末样品干燥后分析测试。X射线激发光源为单色Al Kα (hν = 1486.6 eV) 射线。得到的谱图信号以C1s 284.6 eV校正。
0.07% Pt/r.d-SnO2-ALD, 0.27% Pt/r.d-SnO2-ALD, 0.32% Pt/r.d-SnO2-ALD powder samples were analyzed and tested after drying. The X-ray excitation source is a monochromatic Al Kα (hν = 1486.6eV) ray. The resulting spectral signal is calibrated at C1s 284.6eV.