GH984G不同磷含量锻态合金热变形至真应变为0.69后的组织形貌 (a) 950 °C / 0.01 s-1,(b) 950 °C / 1.0 s-1,(c) 1150 °C / 0.01 s-1,(d) 1150 °C / 1.0 s-1
The OIM maps of the forged alloys after deformation at 950 °C / 0.01 s-1 (a), 950 °C / 1.0 s-1 (b), 1150 °C / 0.01 s-1 (c) and 1150 °C / 1.0 s-1 (d) with the true strain of 0.69.